Fig. 7

Bright-field TEM images of a Pt3Al precipitate in a Pt86:Al14 alloy showing the dissolution of small precipitates at increasing temperatures: (a) 580°C; (b) 870°C (31)

Bright-field TEM images of a Pt3Al precipitate in a Pt86:Al14 alloy showing the dissolution of small precipitates at increasing temperatures: (a) 580°C; (b) 870°C (31)