Fig. 5

Platinum metals recoveries into chlorination solution as a function of initial slurry density (170 g l−1 HCl, chlorination time = 2 hours)

Platinum metals recoveries into chlorination solution as a function of initial slurry density (170 g l−1 HCl, chlorination time = 2 hours)