Fig. 5

Fig. 5

Irreversible CO adsorption after saturation at 90 K over CeO2, Au/CeO2, Rh/CeO2 and Rh–Au/CeO2. The catalysts were heated at the indicated temperatures after CO adsorption at 90 K, then quenched back to 90 K for further data collection